Ferro Frit 4171

Leadless calcium borosilicate frit (was Frit 3271, Frit 1057)

Alternate Names: Frit 1057, Frit 3271, Frit DA4171

OxideAnalysisFormula
CaO11.00%0.487
Na2O12.80%0.513
B2O321.60%0.771
SiO254.60%2.257
Oxide Weight248.43
Formula Weight248.43
If this formula is not unified correctly please contact us.
COLE - Co-efficient of Linear Expansion 9.30
GSPT - Frit Softening Point 558C
MLRG - Frit Melting Range (C) 1040-1100C
GTTM - Glass Transition Temperature 590C

Out Bound Links

In Bound Links


By Tony Hansen

XML for Import into INSIGHT

<?xml version="1.0" encoding="UTF-8"?> <material name="Ferro Frit 4171" descrip="Leadless calcium borosilicate frit (was Frit 3271, Frit 1057)" searchkey="Frit 1057, Frit 3271, Frit DA4171" loi="0.00" casnumber="65997-18-4"> <oxides> <oxide symbol="CaO" name="Calcium Oxide, Calcia" status="" percent="11.000" tolerance=""/> <oxide symbol="Na2O" name="Sodium Oxide, Soda" status="" percent="12.800" tolerance=""/> <oxide symbol="B2O3" name="Boric Oxide" status="" percent="21.600" tolerance=""/> <oxide symbol="SiO2" name="Silicon Dioxide, Silica" status="" percent="54.600" tolerance=""/> </oxides> </material>


Feedback, Suggestions

Your email address

Subject

Your Name

Message


Copyright 2003, 2008, 2015 https://digitalfire.com, All Rights Reserved