Ferro Frit 4125

Low melting high expansion sodium borosilicate fluorine frit

Alternate Names: Ferro Frit 5325

OxideAnalysisFormula
CaO2.36%0.137
K2O2.59%0.089
Na2O14.77%0.774
F2.72%0.465
Al2O37.97%0.254
B2O313.81%0.645
SiO255.77%3.015
Oxide Weight324.87
Formula Weight324.87
If this formula is not unified correctly please contact us.

Was known as Ferro Frit 5325


Out Bound Links

In Bound Links


By Tony Hansen

XML for Import into INSIGHT

<?xml version="1.0" encoding="UTF-8"?> <material name="Ferro Frit 4125" descrip="Low melting high expansion sodium borosilicate fluorine frit" searchkey="Ferro Frit 5325" loi="0.00" casnumber="65997-18-4"> <oxides> <oxide symbol="CaO" name="Calcium Oxide, Calcia" status="" percent="2.360" tolerance=""/> <oxide symbol="K2O" name="Potassium Oxide" status="" percent="2.590" tolerance=""/> <oxide symbol="Na2O" name="Sodium Oxide, Soda" status="" percent="14.770" tolerance=""/> <oxide symbol="F" name="Fluorine" status="" percent="2.720" tolerance=""/> <oxide symbol="Al2O3" name="Aluminum Oxide, Alumina" status="" percent="7.970" tolerance=""/> <oxide symbol="B2O3" name="Boric Oxide" status="" percent="13.810" tolerance=""/> <oxide symbol="SiO2" name="Silicon Dioxide, Silica" status="" percent="55.770" tolerance=""/> </oxides> </material>


Feedback, Suggestions

Your email address

Subject

Your Name

Message


Copyright 2003, 2008, 2015 https://digitalfire.com, All Rights Reserved