Ferro Frit 4113

General purpose hard and versatile borosilicate frit

Alternate Names: Frit KFG 4113, Frit 4712, Frit DA4113

OxideAnalysisFormula
CaO9.28%0.589
K2O3.53%0.133
Na2O4.84%0.278
Al2O310.05%0.351
B2O312.73%0.651
SiO259.58%3.528
Oxide Weight355.96
Formula Weight355.96
If this formula is not unified correctly please contact us.
GSPT - Frit Softening Point 586C
MLRG - Frit Melting Range (C) 1040-1100C
GTTM - Glass Transition Temperature 652C

Formerly Frit 4712. Considered good for developing colors.


Out Bound Links


By Tony Hansen

XML for Import into INSIGHT

<?xml version="1.0" encoding="UTF-8"?> <material name="Ferro Frit 4113" descrip="General purpose hard and versatile borosilicate frit" searchkey="Frit KFG 4113, Frit 4712, Frit DA4113" loi="0.00" casnumber="65997-18-4"> <oxides> <oxide symbol="CaO" name="Calcium Oxide, Calcia" status="" percent="9.280" tolerance=""/> <oxide symbol="K2O" name="Potassium Oxide" status="" percent="3.530" tolerance=""/> <oxide symbol="Na2O" name="Sodium Oxide, Soda" status="" percent="4.840" tolerance=""/> <oxide symbol="Al2O3" name="Aluminum Oxide, Alumina" status="" percent="10.050" tolerance=""/> <oxide symbol="B2O3" name="Boric Oxide" status="" percent="12.730" tolerance=""/> <oxide symbol="SiO2" name="Silicon Dioxide, Silica" status="" percent="59.580" tolerance=""/> </oxides> </material>


Feedback, Suggestions

Your email address

Subject

Your Name

Message


Copyright 2003, 2008, 2015 https://digitalfire.com, All Rights Reserved