Ferro Frit 4112

Calcium Borate Frit

OxideAnalysisFormula
CaO26.25%1.000
Al2O37.03%0.147
B2O349.53%1.521
SiO217.20%0.612
Oxide Weight213.74
Formula Weight213.74
If this formula is not unified correctly please contact us.

Firing Range: 1050 - 1160 C
Chemistry similar to colemanite
No longer manufactured


Out Bound Links

In Bound Links


By Tony Hansen

XML for Import into INSIGHT

<?xml version="1.0" encoding="UTF-8"?> <material name="Ferro Frit 4112" descrip="Calcium Borate Frit" searchkey="" loi="0.00" casnumber="65997-18-4"> <oxides> <oxide symbol="CaO" name="Calcium Oxide, Calcia" status="" percent="26.250" tolerance=""/> <oxide symbol="Al2O3" name="Aluminum Oxide, Alumina" status="" percent="7.030" tolerance=""/> <oxide symbol="B2O3" name="Boric Oxide" status="" percent="49.530" tolerance=""/> <oxide symbol="SiO2" name="Silicon Dioxide, Silica" status="" percent="17.200" tolerance=""/> </oxides> </material>


Feedback, Suggestions

Your email address

Subject

Your Name

Message


Copyright 2003, 2008, 2015 https://digitalfire.com, All Rights Reserved