Ferro Frit 4110

Leadless high expansion high alkali frit, formerly Frit 3110

Alternate Names: Frit KFG 4110, Frit DA4110

Oxide Weight261.01
Formula Weight261.01
If this formula is not unified correctly please contact us.
COLE - Co-efficient of Linear Expansion 8.50
GSPT - Frit Softening Point 575C
MLRG - Frit Melting Range (C) 1000-1060C
GTTM - Glass Transition Temperature 531C

Good for copper blues and manganese purples.
Very similar but not identical to Ferro Frit 3110.
The data sheet at Walker Ceramics 2015 shows a little less SiO2 than this one.

Out Bound Links

In Bound Links

By Tony Hansen

XML for Import into INSIGHT

<?xml version="1.0" encoding="UTF-8"?> <material name="Ferro Frit 4110" descrip="Leadless high expansion high alkali frit, formerly Frit 3110" searchkey="Frit KFG 4110, Frit DA4110" loi="0.00" casnumber="65997-18-4"> <oxides> <oxide symbol="CaO" name="Calcium Oxide, Calcia" status="" percent="6.130" tolerance=""/> <oxide symbol="K2O" name="Potassium Oxide" status="" percent="2.540" tolerance=""/> <oxide symbol="Na2O" name="Sodium Oxide, Soda" status="" percent="15.310" tolerance=""/> <oxide symbol="Al2O3" name="Aluminum Oxide, Alumina" status="" percent="4.200" tolerance=""/> <oxide symbol="B2O3" name="Boric Oxide" status="" percent="2.680" tolerance=""/> <oxide symbol="SiO2" name="Silicon Dioxide, Silica" status="" percent="69.150" tolerance=""/> </oxides> </material>

Feedback, Suggestions

Your email address


Your Name


Copyright 2003, 2008, 2015 https://digitalfire.com, All Rights Reserved