Ferro Frit 4108

Low alumina high CaO boro silicate frit

Alternate Names: Frit 4508, Frit DA4108, Frit KPM 4108

OxideAnalysisFormula
CaO16.68%0.681
Na2O8.64%0.319
Al2O33.12%0.070
B2O319.33%0.636
SiO252.23%1.990
Oxide Weight229.00
Formula Weight229.00
If this formula is not unified correctly please contact us.
GSPT - Frit Softening Point 583C
MLRG - Frit Melting Range (C) 1040-1100C
GTTM - Glass Transition Temperature 618C

Formerly Frit 4508


Out Bound Links

In Bound Links


By Tony Hansen

XML for Import into INSIGHT

<?xml version="1.0" encoding="UTF-8"?> <material name="Ferro Frit 4108" descrip="Low alumina high CaO boro silicate frit" searchkey="Frit 4508, Frit DA4108, Frit KPM 4108" loi="0.00" casnumber="65997-18-4"> <oxides> <oxide symbol="CaO" name="Calcium Oxide, Calcia" status="" percent="16.680" tolerance=""/> <oxide symbol="Na2O" name="Sodium Oxide, Soda" status="" percent="8.640" tolerance=""/> <oxide symbol="Al2O3" name="Aluminum Oxide, Alumina" status="" percent="3.120" tolerance=""/> <oxide symbol="B2O3" name="Boric Oxide" status="" percent="19.330" tolerance=""/> <oxide symbol="SiO2" name="Silicon Dioxide, Silica" status="" percent="52.230" tolerance=""/> </oxides> </material>


Feedback, Suggestions

Your email address

Subject

Your Name

Message


Copyright 2003, 2008, 2015 https://digitalfire.com, All Rights Reserved