Ferro Frit 4101

High expansion sodium borosilicate fluorine frit

Alternate Names: Formerly Ferro Frit 530

OxideAnalysisFormula
CaO1.90%0.079
K2O20.35%0.505
Na2O11.05%0.416
F4.35%0.535
Al2O37.22%0.165
B2O311.18%0.375
SiO243.95%1.708
Oxide Weight233.58
Formula Weight233.58
If this formula is not unified correctly please contact us.

Out Bound Links

In Bound Links


By Tony Hansen

XML for Import into INSIGHT

<?xml version="1.0" encoding="UTF-8"?> <material name="Ferro Frit 4101" descrip="High expansion sodium borosilicate fluorine frit" searchkey="Formerly Ferro Frit 530" loi="0.00" casnumber="65997-18-4"> <oxides> <oxide symbol="CaO" name="Calcium Oxide, Calcia" status="" percent="1.900" tolerance=""/> <oxide symbol="K2O" name="Potassium Oxide" status="" percent="20.350" tolerance=""/> <oxide symbol="Na2O" name="Sodium Oxide, Soda" status="" percent="11.050" tolerance=""/> <oxide symbol="F" name="Fluorine" status="" percent="4.350" tolerance=""/> <oxide symbol="Al2O3" name="Aluminum Oxide, Alumina" status="" percent="7.220" tolerance=""/> <oxide symbol="B2O3" name="Boric Oxide" status="" percent="11.180" tolerance=""/> <oxide symbol="SiO2" name="Silicon Dioxide, Silica" status="" percent="43.950" tolerance=""/> </oxides> </material>


Feedback, Suggestions

Your email address

Subject

Your Name

Message


Copyright 2003, 2008, 2015 https://digitalfire.com, All Rights Reserved