Ferro Frit 4049

High boron low lead frit

OxideAnalysisFormula
BaO0.03%0.001
CaO6.70%0.399
MgO0.23%0.019
K2O7.40%0.262
Na2O4.03%0.217
ZnO0.20%0.008
SrO0.07%0.002
PbO6.17%0.092
B2O324.07%1.154
SiO250.80%2.821
Oxide Weight332.71
Formula Weight332.71
If this formula is not unified correctly please contact us.

Out Bound Links


By Tony Hansen

XML for Import into INSIGHT

<?xml version="1.0" encoding="UTF-8"?> <material name="Ferro Frit 4049" descrip="High boron low lead frit" searchkey="" loi="0.00" casnumber="65997-18-4"> <oxides> <oxide symbol="BaO" name="Barium Oxide, Baria" status="" percent="0.030" tolerance=""/> <oxide symbol="CaO" name="Calcium Oxide, Calcia" status="" percent="6.700" tolerance=""/> <oxide symbol="MgO" name="Magnesium Oxide, Magnesia" status="" percent="0.230" tolerance=""/> <oxide symbol="K2O" name="Potassium Oxide" status="" percent="7.400" tolerance=""/> <oxide symbol="Na2O" name="Sodium Oxide, Soda" status="" percent="4.030" tolerance=""/> <oxide symbol="ZnO" name="Zinc Oxide" status="" percent="0.200" tolerance=""/> <oxide symbol="SrO" name="Strontium Oxide, Strontia" status="" percent="0.070" tolerance=""/> <oxide symbol="PbO" name="Lead Oxide" status="" percent="6.170" tolerance=""/> <oxide symbol="B2O3" name="Boric Oxide" status="" percent="24.070" tolerance=""/> <oxide symbol="SiO2" name="Silicon Dioxide, Silica" status="" percent="50.800" tolerance=""/> </oxides> </material>


Feedback, Suggestions

Your email address

Subject

Your Name

Message


Copyright 2003, 2008, 2015 https://digitalfire.com, All Rights Reserved