Ferro Frit 3831

Barium calcium alkali boron free frit

OxideAnalysisFormula
BaO17.90%0.218
CaO12.20%0.406
K2O12.00%0.238
Na2O4.60%0.138
Al2O310.60%0.194
SiO242.70%1.326
Oxide Weight186.63
Formula Weight186.63
If this formula is not unified correctly please contact us.
COLE - Co-efficient of Linear Expansion 11.90
MLRG - Frit Melting Range (C) 1700F

Out Bound Links

In Bound Links


By Tony Hansen

XML for Import into INSIGHT

<?xml version="1.0" encoding="UTF-8"?> <material name="Ferro Frit 3831" descrip="Barium calcium alkali boron free frit" searchkey="" loi="0.00" casnumber="65997-18-4"> <oxides> <oxide symbol="BaO" name="Barium Oxide, Baria" status="" percent="17.900" tolerance=""/> <oxide symbol="CaO" name="Calcium Oxide, Calcia" status="" percent="12.200" tolerance=""/> <oxide symbol="K2O" name="Potassium Oxide" status="" percent="12.000" tolerance=""/> <oxide symbol="Na2O" name="Sodium Oxide, Soda" status="" percent="4.600" tolerance=""/> <oxide symbol="Al2O3" name="Aluminum Oxide, Alumina" status="" percent="10.600" tolerance=""/> <oxide symbol="SiO2" name="Silicon Dioxide, Silica" status="" percent="42.700" tolerance=""/> </oxides> </material>


Feedback, Suggestions

Your email address

Subject

Your Name

Message


Copyright 2003, 2008, 2015 https://digitalfire.com, All Rights Reserved