Ferro Frit 3824

Leadless zinc frit

OxideAnalysisFormula
CaO4.50%0.189
Na2O9.10%0.346
ZnO16.10%0.466
B2O329.10%0.984
SiO241.20%1.614
Oxide Weight235.42
Formula Weight235.42
If this formula is not unified correctly please contact us.
COLE - Co-efficient of Linear Expansion 8.30
MLRG - Frit Melting Range (C) 1400F

Out Bound Links


By Tony Hansen

XML for Import into INSIGHT

<?xml version="1.0" encoding="UTF-8"?> <material name="Ferro Frit 3824" descrip="Leadless zinc frit" searchkey="" loi="0.00" casnumber="65997-18-4"> <oxides> <oxide symbol="CaO" name="Calcium Oxide, Calcia" status="" percent="4.500" tolerance=""/> <oxide symbol="Na2O" name="Sodium Oxide, Soda" status="" percent="9.100" tolerance=""/> <oxide symbol="ZnO" name="Zinc Oxide" status="" percent="16.100" tolerance=""/> <oxide symbol="B2O3" name="Boric Oxide" status="" percent="29.100" tolerance=""/> <oxide symbol="SiO2" name="Silicon Dioxide, Silica" status="" percent="41.200" tolerance=""/> </oxides> </material>