Zinc alkali borosilicate frit

OxideAnalysisFormula
CaO5.30%0.240
MgO0.50%0.032
K2O8.10%0.219
Na2O5.10%0.209
ZnO9.60%0.300
Al2O313.00%0.324
B2O34.60%0.168
SiO250.88%2.154
ZrO22.90%0.060
Oxide Weight254.36
Formula Weight254.36
If this formula is not unified correctly please contact us.
COLE - Co-efficient of Linear Expansion 8.30
MLRG - Frit Melting Range (C) 1650F

Out Bound Links


By Tony Hansen

XML for Import into INSIGHT

<?xml version="1.0" encoding="UTF-8"?> <material name="Ferro Frit 3820" descrip="Zinc alkali borosilicate frit" searchkey="" loi="0.00" casnumber="65997-18-4"> <oxides> <oxide symbol="CaO" name="Calcium Oxide, Calcia" status="" percent="5.300" tolerance=""/> <oxide symbol="MgO" name="Magnesium Oxide, Magnesia" status="" percent="0.500" tolerance=""/> <oxide symbol="K2O" name="Potassium Oxide" status="" percent="8.100" tolerance=""/> <oxide symbol="Na2O" name="Sodium Oxide, Soda" status="" percent="5.100" tolerance=""/> <oxide symbol="ZnO" name="Zinc Oxide" status="" percent="9.600" tolerance=""/> <oxide symbol="Al2O3" name="Aluminum Oxide, Alumina" status="" percent="13.000" tolerance=""/> <oxide symbol="B2O3" name="Boric Oxide" status="" percent="4.600" tolerance=""/> <oxide symbol="SiO2" name="Silicon Dioxide, Silica" status="" percent="50.880" tolerance=""/> <oxide symbol="ZrO2" name="Zirconium Dioxide" status="" percent="2.900" tolerance=""/> </oxides> </material>


Feedback, Suggestions

Your email address

Subject

Your Name

Message


Copyright 2003, 2008, 2015 https://digitalfire.com, All Rights Reserved