Ferro Frit 3819

Leadless high sodium frit for cone 06-02

OxideAnalysisFormula
CaO0.30%0.018
K2O7.20%0.252
Na2O13.00%0.690
ZnO1.00%0.040
F1.60%0.277
Al2O312.60%0.407
B2O316.60%0.785
SiO247.70%2.613
Oxide Weight329.23
Formula Weight329.23
If this formula is not unified correctly please contact us.
COLE - Co-efficient of Linear Expansion 10.30
GSPT - Frit Softening Point 1400F

Out Bound Links

In Bound Links


By Tony Hansen

XML for Import into INSIGHT

<?xml version="1.0" encoding="UTF-8"?> <material name="Ferro Frit 3819" descrip="Leadless high sodium frit for cone 06-02" searchkey="" loi="0.00" casnumber="65997-18-4"> <oxides> <oxide symbol="CaO" name="Calcium Oxide, Calcia" status="" percent="0.300" tolerance=""/> <oxide symbol="K2O" name="Potassium Oxide" status="" percent="7.200" tolerance=""/> <oxide symbol="Na2O" name="Sodium Oxide, Soda" status="" percent="13.000" tolerance=""/> <oxide symbol="ZnO" name="Zinc Oxide" status="" percent="1.000" tolerance=""/> <oxide symbol="F" name="Fluorine" status="" percent="1.600" tolerance=""/> <oxide symbol="Al2O3" name="Aluminum Oxide, Alumina" status="" percent="12.600" tolerance=""/> <oxide symbol="B2O3" name="Boric Oxide" status="" percent="16.600" tolerance=""/> <oxide symbol="SiO2" name="Silicon Dioxide, Silica" status="" percent="47.700" tolerance=""/> </oxides> </material>


Feedback, Suggestions

Your email address

Subject

Your Name

Message


Copyright 2003, 2008, 2015 https://digitalfire.com, All Rights Reserved