Ferro Frit 3814

Leadless calcium borosilicate frit

OxideAnalysisFormula
CaO16.80%0.674
K2O0.40%0.010
Na2O8.70%0.316
Al2O35.00%0.110
B2O319.30%0.624
SiO249.80%1.866
Oxide Weight225.21
Formula Weight225.21
If this formula is not unified correctly please contact us.
COLE - Co-efficient of Linear Expansion 8.9 x 10-6
MLRG - Frit Melting Range (C) 1500F

Out Bound Links

In Bound Links


By Tony Hansen

XML for Import into INSIGHT

<?xml version="1.0" encoding="UTF-8"?> <material name="Ferro Frit 3814" descrip="Leadless calcium borosilicate frit" searchkey="" loi="0.00" casnumber="65997-18-4"> <oxides> <oxide symbol="CaO" name="Calcium Oxide, Calcia" status="" percent="16.800" tolerance=""/> <oxide symbol="K2O" name="Potassium Oxide" status="" percent="0.400" tolerance=""/> <oxide symbol="Na2O" name="Sodium Oxide, Soda" status="" percent="8.700" tolerance=""/> <oxide symbol="Al2O3" name="Aluminum Oxide, Alumina" status="" percent="5.000" tolerance=""/> <oxide symbol="B2O3" name="Boric Oxide" status="" percent="19.300" tolerance=""/> <oxide symbol="SiO2" name="Silicon Dioxide, Silica" status="" percent="49.800" tolerance=""/> </oxides> </material>


Feedback, Suggestions

Your email address

Subject

Your Name

Message


Copyright 2003, 2008, 2015 https://digitalfire.com, All Rights Reserved