Ferro Frit 3576

Medium lead hobby/artware glaze frit cone 06-04

OxideAnalysisFormula
CaO4.80%0.290
Na2O3.80%0.208
PbO33.00%0.502
Al2O33.50%0.116
B2O313.70%0.668
SiO240.40%2.281
ZrO20.80%0.022
Oxide Weight339.33
Formula Weight339.33
If this formula is not unified correctly please contact us.
COLE - Co-efficient of Linear Expansion 7.10
MLRG - Frit Melting Range (C) 1500F

Out Bound Links


By Tony Hansen

XML for Import into INSIGHT

<?xml version="1.0" encoding="UTF-8"?> <material name="Ferro Frit 3576" descrip="Medium lead hobby/artware glaze frit cone 06-04" searchkey="" loi="0.00" casnumber="65997-18-4"> <oxides> <oxide symbol="CaO" name="Calcium Oxide, Calcia" status="" percent="4.800" tolerance=""/> <oxide symbol="Na2O" name="Sodium Oxide, Soda" status="" percent="3.800" tolerance=""/> <oxide symbol="PbO" name="Lead Oxide" status="" percent="33.000" tolerance=""/> <oxide symbol="Al2O3" name="Aluminum Oxide, Alumina" status="" percent="3.500" tolerance=""/> <oxide symbol="B2O3" name="Boric Oxide" status="" percent="13.700" tolerance=""/> <oxide symbol="SiO2" name="Silicon Dioxide, Silica" status="" percent="40.400" tolerance=""/> <oxide symbol="ZrO2" name="Zirconium Dioxide" status="" percent="0.800" tolerance=""/> </oxides> </material>


Feedback, Suggestions

Your email address

Subject

Your Name

Message


Copyright 2003, 2008, 2015 https://digitalfire.com, All Rights Reserved