Ferro Frit 3563

LEAD BEARING FRIT

OxideAnalysisFormula
CaO5.90%0.290
K2O2.39%0.070
Na2O4.05%0.180
ZnO9.44%0.320
PbO11.33%0.140
Al2O37.40%0.200
B2O36.56%0.260
SiO252.94%2.429
Oxide Weight275.82
Formula Weight275.82
If this formula is not unified correctly please contact us.
COLE - Co-efficient of Linear Expansion 7.7
MLRG - Frit Melting Range (C) 1600F

Out Bound Links

In Bound Links


By Tony Hansen

XML for Import into INSIGHT

<?xml version="1.0" encoding="UTF-8"?> <material name="Ferro Frit 3563" descrip="LEAD BEARING FRIT" searchkey="" loi="0.00" casnumber="65997-18-4"> <oxides> <oxide symbol="CaO" name="Calcium Oxide, Calcia" status="" percent="5.900" tolerance=""/> <oxide symbol="K2O" name="Potassium Oxide" status="" percent="2.390" tolerance=""/> <oxide symbol="Na2O" name="Sodium Oxide, Soda" status="" percent="4.050" tolerance=""/> <oxide symbol="ZnO" name="Zinc Oxide" status="" percent="9.440" tolerance=""/> <oxide symbol="PbO" name="Lead Oxide" status="" percent="11.330" tolerance=""/> <oxide symbol="Al2O3" name="Aluminum Oxide, Alumina" status="" percent="7.400" tolerance=""/> <oxide symbol="B2O3" name="Boric Oxide" status="" percent="6.560" tolerance=""/> <oxide symbol="SiO2" name="Silicon Dioxide, Silica" status="" percent="52.940" tolerance=""/> </oxides> </material>


Feedback, Suggestions

Your email address

Subject

Your Name

Message


Copyright 2003, 2008, 2015 https://digitalfire.com, All Rights Reserved