Ferro Frit 3560

Very low lead zinc barium frit

OxideAnalysisFormula
BaO3.95%0.060
CaO6.99%0.290
MgO2.08%0.120
K2O3.64%0.090
Na2O5.06%0.190
ZnO7.69%0.220
PbO2.88%0.030
Al2O312.70%0.290
B2O32.09%0.070
SiO252.92%2.050
Oxide Weight232.77
Formula Weight232.77
If this formula is not unified correctly please contact us.
COLE - Co-efficient of Linear Expansion 8.6
MLRG - Frit Melting Range (C) 1700F

Out Bound Links


By Tony Hansen

XML for Import into INSIGHT

<?xml version="1.0" encoding="UTF-8"?> <material name="Ferro Frit 3560" descrip="Very low lead zinc barium frit" searchkey="" loi="0.00" casnumber="65997-18-4"> <oxides> <oxide symbol="BaO" name="Barium Oxide, Baria" status="" percent="3.950" tolerance=""/> <oxide symbol="CaO" name="Calcium Oxide, Calcia" status="" percent="6.990" tolerance=""/> <oxide symbol="MgO" name="Magnesium Oxide, Magnesia" status="" percent="2.080" tolerance=""/> <oxide symbol="K2O" name="Potassium Oxide" status="" percent="3.640" tolerance=""/> <oxide symbol="Na2O" name="Sodium Oxide, Soda" status="" percent="5.060" tolerance=""/> <oxide symbol="ZnO" name="Zinc Oxide" status="" percent="7.690" tolerance=""/> <oxide symbol="PbO" name="Lead Oxide" status="" percent="2.880" tolerance=""/> <oxide symbol="Al2O3" name="Aluminum Oxide, Alumina" status="" percent="12.700" tolerance=""/> <oxide symbol="B2O3" name="Boric Oxide" status="" percent="2.090" tolerance=""/> <oxide symbol="SiO2" name="Silicon Dioxide, Silica" status="" percent="52.920" tolerance=""/> </oxides> </material>


Feedback, Suggestions

Your email address

Subject

Your Name

Message


Copyright 2003, 2008, 2015 https://digitalfire.com, All Rights Reserved