Ferro Frit 3516

Lead calcium borosilicate frit

OxideAnalysisFormula
CaO12.30%0.516
K2O1.80%0.045
Na2O1.10%0.042
PbO37.60%0.397
Al2O32.60%0.060
B2O313.00%0.440
SiO231.60%1.238
Oxide Weight235.54
Formula Weight235.54
If this formula is not unified correctly please contact us.
COLE - Co-efficient of Linear Expansion 7.6
MLRG - Frit Melting Range (C) 1400F

Out Bound Links


By Tony Hansen

XML for Import into INSIGHT

<?xml version="1.0" encoding="UTF-8"?> <material name="Ferro Frit 3516" descrip="Lead calcium borosilicate frit" searchkey="" loi="0.00" casnumber="65997-18-4"> <oxides> <oxide symbol="CaO" name="Calcium Oxide, Calcia" status="" percent="12.300" tolerance=""/> <oxide symbol="K2O" name="Potassium Oxide" status="" percent="1.800" tolerance=""/> <oxide symbol="Na2O" name="Sodium Oxide, Soda" status="" percent="1.100" tolerance=""/> <oxide symbol="PbO" name="Lead Oxide" status="" percent="37.600" tolerance=""/> <oxide symbol="Al2O3" name="Aluminum Oxide, Alumina" status="" percent="2.600" tolerance=""/> <oxide symbol="B2O3" name="Boric Oxide" status="" percent="13.000" tolerance=""/> <oxide symbol="SiO2" name="Silicon Dioxide, Silica" status="" percent="31.600" tolerance=""/> </oxides> </material>


Feedback, Suggestions

Your email address

Subject

Your Name

Message


Copyright 2003, 2008, 2015 https://digitalfire.com, All Rights Reserved