Ferro Frit 3509

Low lead calcium silicate frit

OxideAnalysisFormula
CaO10.20%0.578
K2O2.80%0.095
Na2O1.80%0.092
PbO16.50%0.235
Al2O35.80%0.181
B2O38.10%0.370
SiO254.80%2.899
Oxide Weight317.97
Formula Weight317.97
If this formula is not unified correctly please contact us.
COLE - Co-efficient of Linear Expansion 7.10
MLRG - Frit Melting Range (C) 1600F

Out Bound Links

In Bound Links


By Tony Hansen

XML for Import into INSIGHT

<?xml version="1.0" encoding="UTF-8"?> <material name="Ferro Frit 3509" descrip="Low lead calcium silicate frit" searchkey="" loi="0.00" casnumber="65997-18-4"> <oxides> <oxide symbol="CaO" name="Calcium Oxide, Calcia" status="" percent="10.200" tolerance=""/> <oxide symbol="K2O" name="Potassium Oxide" status="" percent="2.800" tolerance=""/> <oxide symbol="Na2O" name="Sodium Oxide, Soda" status="" percent="1.800" tolerance=""/> <oxide symbol="PbO" name="Lead Oxide" status="" percent="16.500" tolerance=""/> <oxide symbol="Al2O3" name="Aluminum Oxide, Alumina" status="" percent="5.800" tolerance=""/> <oxide symbol="B2O3" name="Boric Oxide" status="" percent="8.100" tolerance=""/> <oxide symbol="SiO2" name="Silicon Dioxide, Silica" status="" percent="54.800" tolerance=""/> </oxides> </material>


Feedback, Suggestions

Your email address

Subject

Your Name

Message


Copyright 2003, 2008, 2015 https://digitalfire.com, All Rights Reserved