1-9 | A | B | C | D | E | F | Frits | G | H | I | J | K | L | M | N | O | P | Q | R | S | T | U | V | W | X | Y | Z

Ferro Frit 3497

Oxide Analysis Formula
CaO 9.50% 0.55
K2O 1.50% 0.05
Na2O 2.50% 0.13
PbO 19.00% 0.27
B2O3 5.00% 0.23
Al2O3 5.50% 0.17
SiO2 57.00% 3.05
Oxide Weight 321.84
Formula Weight 321.84

Related Information

Links

Materials Frit
Materials General Frit L-294-J
Hazards Lead in Frits: The Hazards
Suppliers Ferro Corporation
Typecodes Leaded Frit
Frits can contain 1% or 80% PbO so this category can be misleading, check the chemistry to find out.
Typecodes Frit

Data

Co-efficient of Linear Expansion7.20

By Tony Hansen