Ferro Frit 3496

Oxide Analysis Formula
CaO 4.20% 0.27
K2O 1.40% 0.05
Na2O 2.40% 0.14
PbO 33.10% 0.54
B2O3 4.30% 0.22
Al2O3 4.90% 0.17
SiO2 49.70% 2.99
Oxide Weight 361.36
Formula Weight 361.36

Related Information

Links

Materials Frit
Materials Fusion Frit FL-308
Hazards Lead in Frits: The Hazards
Suppliers Ferro Corporation
Typecodes Leaded Frit
Frits can contain 1% or 80% PbO so this category can be misleading, check the chemistry to find out.
Typecodes Frit

Data

Co-efficient of Linear Expansion7.10
Frit Melting Range (C)1450F