Ferro Frit 3490

Oxide Analysis Formula
CaO 0.13% 0.01
K2O 1.52% 0.05
Na2O 3.54% 0.16
PbO 62.00% 0.79
B2O3 5.10% 0.21
Al2O3 2.40% 0.07
SiO2 25.26% 1.19
Oxide Weight 282.88
Formula Weight 282.88

Related Information

Links

Materials Frit
Hazards Lead in Frits: The Hazards
Suppliers Ferro Corporation
Typecodes Leaded Frit
Frits can contain 1% or 80% PbO so this category can be misleading, check the chemistry to find out.