Oxide Analysis Formula
CaO 5.60% 0.25
PbO 67.60% 0.75
SiO2 28.60% 1.18
Oxide Weight 252.80
Formula Weight 252.80

Related Information

Links

Materials Frit
Materials Hommel Frit 574
Materials Frit B300
Hazards Lead in Frits: The Hazards
Suppliers Ferro Corporation
Typecodes Leaded Frit
Frits can contain 1% or 80% PbO so this category can be misleading, check the chemistry to find out.
Typecodes Frit

Data

Co-efficient of Linear Expansion7.30
Frit Softening Point1500F