Ferro Frit 3487

Low lead high calcium frit cone 01-3

OxideAnalysisFormula
CaO14.60%0.679
Na2O3.70%0.156
PbO14.20%0.166
Al2O37.40%0.189
B2O38.20%0.307
SiO251.90%2.252
Oxide Weight260.72
Formula Weight260.72
If this formula is not unified correctly please contact us.

Out Bound Links


By Tony Hansen

XML for Import into INSIGHT

<?xml version="1.0" encoding="UTF-8"?> <material name="Ferro Frit 3487" descrip="Low lead high calcium frit cone 01-3" searchkey="" loi="0.00" casnumber="65997-18-4"> <oxides> <oxide symbol="CaO" name="Calcium Oxide, Calcia" status="" percent="14.600" tolerance=""/> <oxide symbol="Na2O" name="Sodium Oxide, Soda" status="" percent="3.700" tolerance=""/> <oxide symbol="PbO" name="Lead Oxide" status="" percent="14.200" tolerance=""/> <oxide symbol="Al2O3" name="Aluminum Oxide, Alumina" status="" percent="7.400" tolerance=""/> <oxide symbol="B2O3" name="Boric Oxide" status="" percent="8.200" tolerance=""/> <oxide symbol="SiO2" name="Silicon Dioxide, Silica" status="" percent="51.900" tolerance=""/> </oxides> </material>


Feedback, Suggestions

Your email address

Subject

Your Name

Message


Copyright 2003, 2008, 2015 https://digitalfire.com, All Rights Reserved