1-9 | A | B | C | D | E | F | Frits | G | H | I | J | K | L | M | N | O | P | Q | R | S | T | U | V | W | X | Y | Z

Ferro Frit 3482

Oxide Analysis Formula
CaO 3.30% 0.21
K2O 3.90% 0.15
Na2O 2.70% 0.16
PbO 29.10% 0.48
TiO2 9.70% 0.44
B2O3 6.00% 0.31
SiO2 43.10% 2.62
F 2.20% 0.42
Oxide Weight 364.76
Formula Weight 364.76

Notes

Ideal for 06-02 matte and artware/hobby glazes because of the Ti.

Related Information

Links

Materials Frit
Materials Pemco Frit Pb-1151
Materials Hommel Frit 334
Materials Frit
Materials Hommel Frit 27
Hazards Lead in Frits: The Hazards
Suppliers Ferro Corporation
Typecodes Leaded Frit
Frits can contain 1% or 80% PbO so this category can be misleading, check the chemistry to find out.
Typecodes Frit

Data

Co-efficient of Linear Expansion8.30
Frit Melting Range (C)1400F

By Tony Hansen