Ferro Frit 3471

Leaded barium calcium borosilicate frit

OxideAnalysisFormula
BaO15.00%0.253
CaO6.50%0.300
K2O2.60%0.071
Na2O0.50%0.021
PbO30.50%0.354
Al2O33.90%0.099
B2O312.30%0.458
SiO228.70%1.237
Oxide Weight259.05
Formula Weight259.05
If this formula is not unified correctly please contact us.
COLE - Co-efficient of Linear Expansion 8.0
MLRG - Frit Melting Range (C) 1500F

Out Bound Links


By Tony Hansen

XML for Import into INSIGHT

<?xml version="1.0" encoding="UTF-8"?> <material name="Ferro Frit 3471" descrip="Leaded barium calcium borosilicate frit" searchkey="" loi="0.00" casnumber="65997-18-4"> <oxides> <oxide symbol="BaO" name="Barium Oxide, Baria" status="" percent="15.000" tolerance=""/> <oxide symbol="CaO" name="Calcium Oxide, Calcia" status="" percent="6.500" tolerance=""/> <oxide symbol="K2O" name="Potassium Oxide" status="" percent="2.600" tolerance=""/> <oxide symbol="Na2O" name="Sodium Oxide, Soda" status="" percent="0.500" tolerance=""/> <oxide symbol="PbO" name="Lead Oxide" status="" percent="30.500" tolerance=""/> <oxide symbol="Al2O3" name="Aluminum Oxide, Alumina" status="" percent="3.900" tolerance=""/> <oxide symbol="B2O3" name="Boric Oxide" status="" percent="12.300" tolerance=""/> <oxide symbol="SiO2" name="Silicon Dioxide, Silica" status="" percent="28.700" tolerance=""/> </oxides> </material>


Feedback, Suggestions

Your email address

Subject

Your Name

Message


Copyright 2003, 2008, 2015 https://digitalfire.com, All Rights Reserved