Ferro Frit 3470

Oxide Analysis Formula
CaO 5.60% 0.23
Na2O 2.20% 0.08
PbO 41.20% 0.43
ZnO 9.00% 0.26
B2O3 8.50% 0.28
Al2O3 5.80% 0.13
SiO2 27.70% 1.07
Oxide Weight 232.31
Formula Weight 232.31

Related Information

1700F Frit Melt-Off 2: Who is the winner?

Links

Materials Frit
Materials Fusion Frit FZ-241
Hazards Lead in Frits: The Hazards
Suppliers Ferro Corporation
Typecodes Leaded Frit
Frits can contain 1% or 80% PbO so this category can be misleading, check the chemistry to find out.
Typecodes Frit

Data

Co-efficient of Linear Expansion7.5
Frit Melting Range (C)1350F