Ferro Frit 3467

Low Lead High Alumina Glaze Frit

Alternate Names: F3467

OxideAnalysisFormula
CaO8.00%0.489
MgO0.60%0.051
K2O1.70%0.062
Na2O2.40%0.133
PbO17.21%0.265
Al2O39.08%0.306
B2O34.50%0.222
SiO256.53%3.228
Oxide Weight343.29
Formula Weight343.29
If this formula is not unified correctly please contact us.
COLE - Co-efficient of Linear Expansion 6.80
MLRG - Frit Melting Range (C) 1700F

Used in all-fritted refire sanitary ware glazes cone 3-5.
Made from silica, borax, calcium, soda, potash and clay.


Out Bound Links

In Bound Links


By Tony Hansen

XML for Import into INSIGHT

<?xml version="1.0" encoding="UTF-8"?> <material name="Ferro Frit 3467" descrip="Low Lead High Alumina Glaze Frit" searchkey="F3467" loi="0.00" casnumber="65997-18-4"> <oxides> <oxide symbol="CaO" name="Calcium Oxide, Calcia" status="" percent="8.000" tolerance=""/> <oxide symbol="MgO" name="Magnesium Oxide, Magnesia" status="" percent="0.600" tolerance=""/> <oxide symbol="K2O" name="Potassium Oxide" status="" percent="1.700" tolerance=""/> <oxide symbol="Na2O" name="Sodium Oxide, Soda" status="" percent="2.400" tolerance=""/> <oxide symbol="PbO" name="Lead Oxide" status="" percent="17.210" tolerance=""/> <oxide symbol="Al2O3" name="Aluminum Oxide, Alumina" status="" percent="9.080" tolerance=""/> <oxide symbol="B2O3" name="Boric Oxide" status="" percent="4.500" tolerance=""/> <oxide symbol="SiO2" name="Silicon Dioxide, Silica" status="" percent="56.530" tolerance=""/> </oxides> </material>