Ferro Frit 3466

Low lead, low boron, low alumina glaze frit cone 2-7

OxideAnalysisFormula
BaO1.50%0.032
CaO7.10%0.417
K2O1.40%0.049
Na2O2.70%0.143
ZnO2.40%0.097
PbO17.70%0.261
Al2O38.90%0.287
B2O35.60%0.265
SiO252.70%2.889
Oxide Weight329.45
Formula Weight329.45
If this formula is not unified correctly please contact us.
COLE - Co-efficient of Linear Expansion 7.2
MLRG - Frit Melting Range (C) 1500F

Out Bound Links


By Tony Hansen

XML for Import into INSIGHT

<?xml version="1.0" encoding="UTF-8"?> <material name="Ferro Frit 3466" descrip="Low lead, low boron, low alumina glaze frit cone 2-7" searchkey="" loi="0.00" casnumber="65997-18-4"> <oxides> <oxide symbol="BaO" name="Barium Oxide, Baria" status="" percent="1.500" tolerance=""/> <oxide symbol="CaO" name="Calcium Oxide, Calcia" status="" percent="7.100" tolerance=""/> <oxide symbol="K2O" name="Potassium Oxide" status="" percent="1.400" tolerance=""/> <oxide symbol="Na2O" name="Sodium Oxide, Soda" status="" percent="2.700" tolerance=""/> <oxide symbol="ZnO" name="Zinc Oxide" status="" percent="2.400" tolerance=""/> <oxide symbol="PbO" name="Lead Oxide" status="" percent="17.700" tolerance=""/> <oxide symbol="Al2O3" name="Aluminum Oxide, Alumina" status="" percent="8.900" tolerance=""/> <oxide symbol="B2O3" name="Boric Oxide" status="" percent="5.600" tolerance=""/> <oxide symbol="SiO2" name="Silicon Dioxide, Silica" status="" percent="52.700" tolerance=""/> </oxides> </material>


Feedback, Suggestions

Your email address

Subject

Your Name

Message


Copyright 2003, 2008, 2015 https://digitalfire.com, All Rights Reserved