Ferro Frit 3465

Low lead high borax frit cone 08-02

OxideAnalysisFormula
CaO6.50%0.307
Na2O14.40%0.616
PbO6.40%0.076
B2O320.20%0.770
SiO252.50%2.318
Oxide Weight265.40
Formula Weight265.40
If this formula is not unified correctly please contact us.
COLE - Co-efficient of Linear Expansion 9.70
MLRG - Frit Melting Range (C) 1600F

Out Bound Links


By Tony Hansen

XML for Import into INSIGHT

<?xml version="1.0" encoding="UTF-8"?> <material name="Ferro Frit 3465" descrip="Low lead high borax frit cone 08-02" searchkey="" loi="0.00" casnumber="65997-18-4"> <oxides> <oxide symbol="CaO" name="Calcium Oxide, Calcia" status="" percent="6.500" tolerance=""/> <oxide symbol="Na2O" name="Sodium Oxide, Soda" status="" percent="14.400" tolerance=""/> <oxide symbol="PbO" name="Lead Oxide" status="" percent="6.400" tolerance=""/> <oxide symbol="B2O3" name="Boric Oxide" status="" percent="20.200" tolerance=""/> <oxide symbol="SiO2" name="Silicon Dioxide, Silica" status="" percent="52.500" tolerance=""/> </oxides> </material>


Feedback, Suggestions

Your email address

Subject

Your Name

Message


Copyright 2003, 2008, 2015 https://digitalfire.com, All Rights Reserved