Ferro Frit 3457

Leaded calcium boron free frit

OxideAnalysisFormula
CaO6.91%0.350
Na2O0.65%0.030
PbO48.68%0.620
Al2O319.02%0.530
SiO224.74%1.170
Oxide Weight284.29
Formula Weight284.29
If this formula is not unified correctly please contact us.
COLE - Co-efficient of Linear Expansion 7.6
MLRG - Frit Melting Range (C) 1350F

Out Bound Links


By Tony Hansen

XML for Import into INSIGHT

<?xml version="1.0" encoding="UTF-8"?> <material name="Ferro Frit 3457" descrip="Leaded calcium boron free frit" searchkey="" loi="0.00" casnumber="65997-18-4"> <oxides> <oxide symbol="CaO" name="Calcium Oxide, Calcia" status="" percent="6.910" tolerance=""/> <oxide symbol="Na2O" name="Sodium Oxide, Soda" status="" percent="0.650" tolerance=""/> <oxide symbol="PbO" name="Lead Oxide" status="" percent="48.680" tolerance=""/> <oxide symbol="Al2O3" name="Aluminum Oxide, Alumina" status="" percent="19.020" tolerance=""/> <oxide symbol="SiO2" name="Silicon Dioxide, Silica" status="" percent="24.740" tolerance=""/> </oxides> </material>


Feedback, Suggestions

Your email address

Subject

Your Name

Message


Copyright 2003, 2008, 2015 https://digitalfire.com, All Rights Reserved