Ferro Frit 3453

Lead monoborate frit

OxideAnalysisFormula
PbO86.70%1.000
B2O311.70%0.433
SiO21.60%0.069
Oxide Weight257.44
Formula Weight257.44
If this formula is not unified correctly please contact us.
COLE - Co-efficient of Linear Expansion 6.8
MLRG - Frit Melting Range (C) 850F

Out Bound Links


By Tony Hansen

XML for Import into INSIGHT

<?xml version="1.0" encoding="UTF-8"?> <material name="Ferro Frit 3453" descrip="Lead monoborate frit" searchkey="" loi="0.00" casnumber="65997-18-4"> <oxides> <oxide symbol="PbO" name="Lead Oxide" status="" percent="86.700" tolerance=""/> <oxide symbol="B2O3" name="Boric Oxide" status="" percent="11.700" tolerance=""/> <oxide symbol="SiO2" name="Silicon Dioxide, Silica" status="" percent="1.600" tolerance=""/> </oxides> </material>


Feedback, Suggestions

Your email address

Subject

Your Name

Message


Copyright 2003, 2008, 2015 https://digitalfire.com, All Rights Reserved