Ferro Frit 3419

High lead borosilicate glaze frit cond 08-02

Alternate Names: F3419

OxideAnalysisFormula
Na2O6.40%0.280
PbO59.20%0.720
B2O314.50%0.565
SiO219.90%0.899
Oxide Weight271.40
Formula Weight271.40
If this formula is not unified correctly please contact us.
COLE - Co-efficient of Linear Expansion 8.2 x 10-6
MLRG - Frit Melting Range (C) 1400F

Out Bound Links

In Bound Links


By Tony Hansen

XML for Import into INSIGHT

<?xml version="1.0" encoding="UTF-8"?> <material name="Ferro Frit 3419" descrip="High lead borosilicate glaze frit cond 08-02" searchkey="F3419" loi="0.00" casnumber="65997-18-4"> <oxides> <oxide symbol="Na2O" name="Sodium Oxide, Soda" status="" percent="6.400" tolerance=""/> <oxide symbol="PbO" name="Lead Oxide" status="" percent="59.200" tolerance=""/> <oxide symbol="B2O3" name="Boric Oxide" status="" percent="14.500" tolerance=""/> <oxide symbol="SiO2" name="Silicon Dioxide, Silica" status="" percent="19.900" tolerance=""/> </oxides> </material>


Feedback, Suggestions

Your email address

Subject

Your Name

Message


Copyright 2003, 2008, 2015 https://digitalfire.com, All Rights Reserved