Ferro Frit 3417

Leaded frit for all fritted glazes cone 06-01

OxideAnalysisFormula
CaO4.50%0.307
K2O1.90%0.077
Na2O1.50%0.093
PbO30.50%0.523
Al2O33.00%0.113
B2O312.60%0.693
SiO243.60%2.777
ZrO22.40%0.075
Oxide Weight382.81
Formula Weight382.81
If this formula is not unified correctly please contact us.
COLE - Co-efficient of Linear Expansion 6.7
MLRG - Frit Melting Range (C) 1400F

Out Bound Links


By Tony Hansen

XML for Import into INSIGHT

<?xml version="1.0" encoding="UTF-8"?> <material name="Ferro Frit 3417" descrip="Leaded frit for all fritted glazes cone 06-01" searchkey="" loi="0.00" casnumber="65997-18-4"> <oxides> <oxide symbol="CaO" name="Calcium Oxide, Calcia" status="" percent="4.500" tolerance=""/> <oxide symbol="K2O" name="Potassium Oxide" status="" percent="1.900" tolerance=""/> <oxide symbol="Na2O" name="Sodium Oxide, Soda" status="" percent="1.500" tolerance=""/> <oxide symbol="PbO" name="Lead Oxide" status="" percent="30.500" tolerance=""/> <oxide symbol="Al2O3" name="Aluminum Oxide, Alumina" status="" percent="3.000" tolerance=""/> <oxide symbol="B2O3" name="Boric Oxide" status="" percent="12.600" tolerance=""/> <oxide symbol="SiO2" name="Silicon Dioxide, Silica" status="" percent="43.600" tolerance=""/> <oxide symbol="ZrO2" name="Zirconium Dioxide" status="" percent="2.400" tolerance=""/> </oxides> </material>


Feedback, Suggestions

Your email address

Subject

Your Name

Message


Copyright 2003, 2008, 2015 https://digitalfire.com, All Rights Reserved