Ferro Frit 3396

Lead alkali frit

OxideAnalysisFormula
Na2O9.40%0.503
PbO33.50%0.497
B2O321.00%1.000
SiO236.10%1.991
Oxide Weight331.45
Formula Weight331.45
If this formula is not unified correctly please contact us.
COLE - Co-efficient of Linear Expansion 9.3 x 10-6 (50-450C)
MLRG - Frit Melting Range (C) 1300F

Out Bound Links


By Tony Hansen

XML for Import into INSIGHT

<?xml version="1.0" encoding="UTF-8"?> <material name="Ferro Frit 3396" descrip="Lead alkali frit" searchkey="" loi="0.00" casnumber="65997-18-4"> <oxides> <oxide symbol="Na2O" name="Sodium Oxide, Soda" status="" percent="9.400" tolerance=""/> <oxide symbol="PbO" name="Lead Oxide" status="" percent="33.500" tolerance=""/> <oxide symbol="B2O3" name="Boric Oxide" status="" percent="21.000" tolerance=""/> <oxide symbol="SiO2" name="Silicon Dioxide, Silica" status="" percent="36.100" tolerance=""/> </oxides> </material>


Feedback, Suggestions

Your email address

Subject

Your Name

Message


Copyright 2003, 2008, 2015 https://digitalfire.com, All Rights Reserved