Ferro Frit 3386

Oxide Analysis Formula
K2O 0.30% 0.02
Na2O 0.60% 0.06
PbO 35.70% 0.93
B2O3 16.30% 1.36
Al2O3 0.30% 0.02
SiO2 46.80% 4.51
Oxide Weight 578.68
Formula Weight 578.68

Related Information

Links

Materials Frit
Hazards Lead in Frits: The Hazards
Suppliers Ferro Corporation
Typecodes Leaded Frit
Frits can contain 1% or 80% PbO so this category can be misleading, check the chemistry to find out.
Typecodes Frit

Data

Co-efficient of Linear Expansion9.70
Co-efficient of Linear Expansion9.7 x 10-6