Ferro Frit 3379

Lead silicate frit

OxideAnalysisFormula
PbO89.79%1.000
SiO210.20%0.422
Oxide Weight248.56
Formula Weight248.56
If this formula is not unified correctly please contact us.

Has more PbO than a lead monosilicate.


Out Bound Links


By Tony Hansen

XML for Import into INSIGHT

<?xml version="1.0" encoding="UTF-8"?> <material name="Ferro Frit 3379" descrip="Lead silicate frit" searchkey="" loi="0.00" casnumber="65997-18-4"> <oxides> <oxide symbol="PbO" name="Lead Oxide" status="" percent="89.797" tolerance=""/> <oxide symbol="SiO2" name="Silicon Dioxide, Silica" status="" percent="10.203" tolerance=""/> </oxides> </material>


Feedback, Suggestions

Your email address

Subject

Your Name

Message


Copyright 2003, 2008, 2015 https://digitalfire.com, All Rights Reserved