Ferro Frit 3377

Lead:silica 1:1 ratio frit (lead monosilicate)

Formula: PbO.SiO2

OxideAnalysisFormula
PbO78.79%1.000
SiO221.21%1.000
Oxide Weight283.28
Formula Weight283.28
If this formula is not unified correctly please contact us.

Out Bound Links

In Bound Links


By Tony Hansen

XML for Import into INSIGHT

<?xml version="1.0" encoding="UTF-8"?> <material name="Ferro Frit 3377" descrip="Lead:silica 1:1 ratio frit (lead monosilicate)" searchkey="" loi="0.00" casnumber="65997-18-4"> <oxides> <oxide symbol="PbO" name="Lead Oxide" status="" percent="78.790" tolerance=""/> <oxide symbol="SiO2" name="Silicon Dioxide, Silica" status="" percent="21.210" tolerance=""/> </oxides> </material>


Feedback, Suggestions

Your email address

Subject

Your Name

Message


Copyright 2003, 2008, 2015 https://digitalfire.com, All Rights Reserved