Ferro Frit 3327

Alternate Names: F3327

Oxide Analysis Formula
PbO 85.00% 1.00
SiO2 15.00% 0.66
Oxide Weight 262.59
Formula Weight 262.59

Related Information

Links

Materials Frit
Materials Lead Monosilicate Frit
Hazards Lead in Frits: The Hazards
Suppliers Ferro Corporation
Typecodes Leaded Frit
Frits can contain 1% or 80% PbO so this category can be misleading, check the chemistry to find out.
Typecodes Frit

By Tony Hansen