Ferro Frit 3304

Alternate Names: F3304

Oxide Analysis Formula
Na2O 1.10% 0.07
PbO 54.40% 0.93
Al2O3 4.00% 0.15
SiO2 40.50% 2.58
Oxide Weight 382.45
Formula Weight 382.45

Notes

Made from flint, soda, clay and lead.

Related Information

Links

Materials Frit
Materials Hommel Frit 61
Hazards Lead in Frits: The Hazards
Suppliers Ferro Corporation
Typecodes Leaded Frit
Frits can contain 1% or 80% PbO so this category can be misleading, check the chemistry to find out.
Typecodes Frit

Data

Co-efficient of Linear Expansion6.6 x 10-6
Frit Melting Range (C)1500F