Ferro Frit 3292

Strontium frit all or partially fritted clear glazes

Alternate Names: F3292

OxideAnalysisFormula
CaO10.53%0.540
Li2O0.42%0.041
MgO0.70%0.050
K2O3.14%0.096
Na2O3.01%0.140
SrO4.83%0.134
Al2O310.76%0.303
B2O35.75%0.238
SiO260.86%2.913
Oxide Weight287.63
Formula Weight287.63
If this formula is not unified correctly please contact us.
COLE - Co-efficient of Linear Expansion 7.62
GSPT - Frit Softening Point 1650-1900F

This is a USA pottery frit, Ferro now calls it Frit 3292-2.

Useful addition to first fire sanitary ware. Balanced, can make up the bulk of a recipe.


Out Bound Links


By Tony Hansen

XML for Import into INSIGHT

<?xml version="1.0" encoding="UTF-8"?> <material name="Ferro Frit 3292" descrip="Strontium frit all or partially fritted clear glazes" searchkey="F3292" loi="0.00" casnumber="65997-18-4"> <oxides> <oxide symbol="CaO" name="Calcium Oxide, Calcia" status="" percent="10.530" tolerance=""/> <oxide symbol="Li2O" name="Lithium Oxide, Lithia" status="" percent="0.420" tolerance=""/> <oxide symbol="MgO" name="Magnesium Oxide, Magnesia" status="" percent="0.700" tolerance=""/> <oxide symbol="K2O" name="Potassium Oxide" status="" percent="3.140" tolerance=""/> <oxide symbol="Na2O" name="Sodium Oxide, Soda" status="" percent="3.010" tolerance=""/> <oxide symbol="SrO" name="Strontium Oxide, Strontia" status="" percent="4.830" tolerance=""/> <oxide symbol="Al2O3" name="Aluminum Oxide, Alumina" status="" percent="10.760" tolerance=""/> <oxide symbol="B2O3" name="Boric Oxide" status="" percent="5.750" tolerance=""/> <oxide symbol="SiO2" name="Silicon Dioxide, Silica" status="" percent="60.860" tolerance=""/> </oxides> </material>


Feedback, Suggestions

Your email address

Subject

Your Name

Message


Copyright 2003, 2008, 2015 https://digitalfire.com, All Rights Reserved