Ferro Frit 3291

Magnesia frit for vitrified bonded abrasives

OxideAnalysisFormula
CaO2.10%0.125
MgO10.60%0.875
Al2O313.20%0.431
B2O328.80%1.377
SiO245.30%2.509
Oxide Weight332.82
Formula Weight332.82
If this formula is not unified correctly please contact us.
COLE - Co-efficient of Linear Expansion 3.90
MLRG - Frit Melting Range (C) 1900F

Out Bound Links

In Bound Links


By Tony Hansen

XML for Import into INSIGHT

<?xml version="1.0" encoding="UTF-8"?> <material name="Ferro Frit 3291" descrip="Magnesia frit for vitrified bonded abrasives" searchkey="" loi="0.00" casnumber="65997-18-4"> <oxides> <oxide symbol="CaO" name="Calcium Oxide, Calcia" status="" percent="2.100" tolerance=""/> <oxide symbol="MgO" name="Magnesium Oxide, Magnesia" status="" percent="10.600" tolerance=""/> <oxide symbol="Al2O3" name="Aluminum Oxide, Alumina" status="" percent="13.200" tolerance=""/> <oxide symbol="B2O3" name="Boric Oxide" status="" percent="28.800" tolerance=""/> <oxide symbol="SiO2" name="Silicon Dioxide, Silica" status="" percent="45.300" tolerance=""/> </oxides> </material>


Feedback, Suggestions

Your email address

Subject

Your Name

Message


Copyright 2003, 2008, 2015 https://digitalfire.com, All Rights Reserved