Ferro Frit 3286

Strontium fluxed all fritted leadless clear glaze

OxideAnalysisFormula
CaO11.10%0.575
K2O3.40%0.105
Na2O1.70%0.080
SrO8.60%0.241
Al2O36.20%0.177
B2O38.80%0.367
SiO260.20%2.909
Oxide Weight290.37
Formula Weight290.37
If this formula is not unified correctly please contact us.
COLE - Co-efficient of Linear Expansion 7.5
MLRG - Frit Melting Range (C) 1750F

Out Bound Links


By Tony Hansen

XML for Import into INSIGHT

<?xml version="1.0" encoding="UTF-8"?> <material name="Ferro Frit 3286" descrip="Strontium fluxed all fritted leadless clear glaze" searchkey="" loi="0.00" casnumber="65997-18-4"> <oxides> <oxide symbol="CaO" name="Calcium Oxide, Calcia" status="" percent="11.100" tolerance=""/> <oxide symbol="K2O" name="Potassium Oxide" status="" percent="3.400" tolerance=""/> <oxide symbol="Na2O" name="Sodium Oxide, Soda" status="" percent="1.700" tolerance=""/> <oxide symbol="SrO" name="Strontium Oxide, Strontia" status="" percent="8.600" tolerance=""/> <oxide symbol="Al2O3" name="Aluminum Oxide, Alumina" status="" percent="6.200" tolerance=""/> <oxide symbol="B2O3" name="Boric Oxide" status="" percent="8.800" tolerance=""/> <oxide symbol="SiO2" name="Silicon Dioxide, Silica" status="" percent="60.200" tolerance=""/> </oxides> </material>


Feedback, Suggestions

Your email address

Subject

Your Name

Message


Copyright 2003, 2008, 2015 https://digitalfire.com, All Rights Reserved