Ferro Frit 3270

Borosilicate cone 06-04 frit for cobalt colors

OxideAnalysisFormula
CaO8.50%0.462
K2O5.40%0.175
Na2O7.40%0.364
Al2O38.30%0.248
B2O322.61%0.990
SiO247.79%2.423
Oxide Weight304.70
Formula Weight304.70
If this formula is not unified correctly please contact us.
COLE - Co-efficient of Linear Expansion 8.79
MLRG - Frit Melting Range (C) 1500-1600F

This is a USA pottery frit, Ferro now calls it Frit 3270-2.
It has higher boron, lower alkali and much higher CaO than Frit 3269. The alkali is still significant enough to drive the thermal expansion fairly high.


Out Bound Links

In Bound Links


By Tony Hansen

XML for Import into INSIGHT

<?xml version="1.0" encoding="UTF-8"?> <material name="Ferro Frit 3270" descrip="Borosilicate cone 06-04 frit for cobalt colors" searchkey="" loi="0.00" casnumber="65997-18-4"> <oxides> <oxide symbol="CaO" name="Calcium Oxide, Calcia" status="" percent="8.500" tolerance=""/> <oxide symbol="K2O" name="Potassium Oxide" status="" percent="5.400" tolerance=""/> <oxide symbol="Na2O" name="Sodium Oxide, Soda" status="" percent="7.400" tolerance=""/> <oxide symbol="Al2O3" name="Aluminum Oxide, Alumina" status="" percent="8.300" tolerance=""/> <oxide symbol="B2O3" name="Boric Oxide" status="" percent="22.610" tolerance=""/> <oxide symbol="SiO2" name="Silicon Dioxide, Silica" status="" percent="47.790" tolerance=""/> </oxides> </material>


Feedback, Suggestions

Your email address

Subject

Your Name

Message


Copyright 2003, 2008, 2015 https://digitalfire.com, All Rights Reserved