Ferro Frit 3264

Leadless high sodium borosilicate

OxideAnalysisFormula
CaO0.10%0.005
MgO0.10%0.007
Na2O20.90%0.988
Al2O36.70%0.192
B2O321.10%0.888
SiO251.10%2.491
Oxide Weight292.95
Formula Weight292.95
If this formula is not unified correctly please contact us.
COLE - Co-efficient of Linear Expansion 11.0 x 10-6 (50-450C)
MLRG - Frit Melting Range (C) 1400F

Out Bound Links

In Bound Links


By Tony Hansen

XML for Import into INSIGHT

<?xml version="1.0" encoding="UTF-8"?> <material name="Ferro Frit 3264" descrip="Leadless high sodium borosilicate" searchkey="" loi="0.00" casnumber="65997-18-4"> <oxides> <oxide symbol="CaO" name="Calcium Oxide, Calcia" status="" percent="0.100" tolerance=""/> <oxide symbol="MgO" name="Magnesium Oxide, Magnesia" status="" percent="0.100" tolerance=""/> <oxide symbol="Na2O" name="Sodium Oxide, Soda" status="" percent="20.900" tolerance=""/> <oxide symbol="Al2O3" name="Aluminum Oxide, Alumina" status="" percent="6.700" tolerance=""/> <oxide symbol="B2O3" name="Boric Oxide" status="" percent="21.100" tolerance=""/> <oxide symbol="SiO2" name="Silicon Dioxide, Silica" status="" percent="51.100" tolerance=""/> </oxides> </material>


Feedback, Suggestions

Your email address

Subject

Your Name

Message


Copyright 2003, 2008, 2015 https://digitalfire.com, All Rights Reserved