Ferro Frit 3240

Zinc barium artware and tile glaze frit

Alternate Names: L-17662B

OxideAnalysisFormula
BaO7.90%0.107
CaO8.80%0.326
K2O0.60%0.013
Na2O4.50%0.151
ZnO15.80%0.403
F1.90%0.208
Al2O30.90%0.018
B2O310.00%0.298
SiO239.50%1.365
ZrO210.20%0.172
Oxide Weight207.91
Formula Weight207.91
If this formula is not unified correctly please contact us.
COLE - Co-efficient of Linear Expansion 8.60
MLRG - Frit Melting Range (C) 1500F

Out Bound Links

In Bound Links


By Tony Hansen

XML for Import into INSIGHT

<?xml version="1.0" encoding="UTF-8"?> <material name="Ferro Frit 3240" descrip="Zinc barium artware and tile glaze frit" searchkey="L-17662B" loi="0.00" casnumber="65997-18-4"> <oxides> <oxide symbol="BaO" name="Barium Oxide, Baria" status="" percent="7.900" tolerance=""/> <oxide symbol="CaO" name="Calcium Oxide, Calcia" status="" percent="8.800" tolerance=""/> <oxide symbol="K2O" name="Potassium Oxide" status="" percent="0.600" tolerance=""/> <oxide symbol="Na2O" name="Sodium Oxide, Soda" status="" percent="4.500" tolerance=""/> <oxide symbol="ZnO" name="Zinc Oxide" status="" percent="15.800" tolerance=""/> <oxide symbol="F" name="Fluorine" status="" percent="1.900" tolerance=""/> <oxide symbol="Al2O3" name="Aluminum Oxide, Alumina" status="" percent="0.900" tolerance=""/> <oxide symbol="B2O3" name="Boric Oxide" status="" percent="10.000" tolerance=""/> <oxide symbol="SiO2" name="Silicon Dioxide, Silica" status="" percent="39.500" tolerance=""/> <oxide symbol="ZrO2" name="Zirconium Dioxide" status="" percent="10.200" tolerance=""/> </oxides> </material>


Feedback, Suggestions

Your email address

Subject

Your Name

Message


Copyright 2003, 2008, 2015 https://digitalfire.com, All Rights Reserved