Ferro Frit 3230

Very high alkaline frit for copper blue, manganese purples

OxideAnalysisFormula
BaO2.04%0.028
K2O11.10%0.248
Na2O18.92%0.641
ZnO3.21%0.083
SiO264.71%2.263
Oxide Weight210.13
Formula Weight210.13
If this formula is not unified correctly please contact us.

Mechanisms

Out Bound Links


By Tony Hansen

XML for Import into INSIGHT

<?xml version="1.0" encoding="UTF-8"?> <material name="Ferro Frit 3230" descrip="Very high alkaline frit for copper blue, manganese purples" searchkey="" loi="0.00" casnumber="65997-18-4"> <oxides> <oxide symbol="BaO" name="Barium Oxide, Baria" status="" percent="2.040" tolerance=""/> <oxide symbol="K2O" name="Potassium Oxide" status="" percent="11.107" tolerance=""/> <oxide symbol="Na2O" name="Sodium Oxide, Soda" status="" percent="18.924" tolerance=""/> <oxide symbol="ZnO" name="Zinc Oxide" status="" percent="3.212" tolerance=""/> <oxide symbol="SiO2" name="Silicon Dioxide, Silica" status="" percent="64.717" tolerance=""/> </oxides> </material>


Feedback, Suggestions

Your email address

Subject

Your Name

Message


Copyright 2003, 2008, 2015 https://digitalfire.com, All Rights Reserved