Ferro Frit 3227

For low temperature vitreous bonding in metals industry

Alternate Names: F3227 Frit, F3227

OxideAnalysisFormula
K2O4.10%0.163
Na2O13.90%0.837
Al2O315.60%0.571
B2O328.50%1.530
SiO237.90%2.356
Oxide Weight373.53
Formula Weight373.53
If this formula is not unified correctly please contact us.
COLE - Co-efficient of Linear Expansion 9.8
MLRG - Frit Melting Range (C) 1300F

Out Bound Links

In Bound Links


By Tony Hansen

XML for Import into INSIGHT

<?xml version="1.0" encoding="UTF-8"?> <material name="Ferro Frit 3227" descrip="For low temperature vitreous bonding in metals industry" searchkey="F3227 Frit, F3227" loi="0.00" casnumber="65997-18-4"> <oxides> <oxide symbol="K2O" name="Potassium Oxide" status="" percent="4.100" tolerance=""/> <oxide symbol="Na2O" name="Sodium Oxide, Soda" status="" percent="13.900" tolerance=""/> <oxide symbol="Al2O3" name="Aluminum Oxide, Alumina" status="" percent="15.600" tolerance=""/> <oxide symbol="B2O3" name="Boric Oxide" status="" percent="28.500" tolerance=""/> <oxide symbol="SiO2" name="Silicon Dioxide, Silica" status="" percent="37.900" tolerance=""/> </oxides> </material>


Feedback, Suggestions

Your email address

Subject

Your Name

Message


Copyright 2003, 2008, 2015 https://digitalfire.com, All Rights Reserved