Ferro Frit 3226

Leadless vitrified bonded abrasives frit

OxideAnalysisFormula
CaO2.90%0.305
Na2O7.30%0.695
Al2O31.00%0.058
B2O336.30%3.078
SiO252.50%5.156
Oxide Weight590.20
Formula Weight590.20
If this formula is not unified correctly please contact us.
COLE - Co-efficient of Linear Expansion 6.30
MLRG - Frit Melting Range (C) 1450F

Out Bound Links

In Bound Links


By Tony Hansen

XML for Import into INSIGHT

<?xml version="1.0" encoding="UTF-8"?> <material name="Ferro Frit 3226" descrip="Leadless vitrified bonded abrasives frit" searchkey="" loi="0.00" casnumber="65997-18-4"> <oxides> <oxide symbol="CaO" name="Calcium Oxide, Calcia" status="" percent="2.900" tolerance=""/> <oxide symbol="Na2O" name="Sodium Oxide, Soda" status="" percent="7.300" tolerance=""/> <oxide symbol="Al2O3" name="Aluminum Oxide, Alumina" status="" percent="1.000" tolerance=""/> <oxide symbol="B2O3" name="Boric Oxide" status="" percent="36.300" tolerance=""/> <oxide symbol="SiO2" name="Silicon Dioxide, Silica" status="" percent="52.500" tolerance=""/> </oxides> </material>


Feedback, Suggestions

Your email address

Subject

Your Name

Message


Copyright 2003, 2008, 2015 https://digitalfire.com, All Rights Reserved