Ferro Frit 3225

Low expansion cone 04 frit for vitrified bonded abrasives

OxideAnalysisFormula
CaO0.30%0.066
MgO0.20%0.061
Na2O4.40%0.873
Al2O38.20%0.989
B2O321.90%3.871
SiO265.00%13.307
Oxide Weight1230.34
Formula Weight1230.34
If this formula is not unified correctly please contact us.
COLE - Co-efficient of Linear Expansion 5.00
MLRG - Frit Melting Range (C) 1650

Out Bound Links


By Tony Hansen

XML for Import into INSIGHT

<?xml version="1.0" encoding="UTF-8"?> <material name="Ferro Frit 3225" descrip="Low expansion cone 04 frit for vitrified bonded abrasives" searchkey="" loi="0.00" casnumber="65997-18-4"> <oxides> <oxide symbol="CaO" name="Calcium Oxide, Calcia" status="" percent="0.300" tolerance=""/> <oxide symbol="MgO" name="Magnesium Oxide, Magnesia" status="" percent="0.200" tolerance=""/> <oxide symbol="Na2O" name="Sodium Oxide, Soda" status="" percent="4.400" tolerance=""/> <oxide symbol="Al2O3" name="Aluminum Oxide, Alumina" status="" percent="8.200" tolerance=""/> <oxide symbol="B2O3" name="Boric Oxide" status="" percent="21.900" tolerance=""/> <oxide symbol="SiO2" name="Silicon Dioxide, Silica" status="" percent="65.000" tolerance=""/> </oxides> </material>


Feedback, Suggestions

Your email address

Subject

Your Name

Message


Copyright 2003, 2008, 2015 https://digitalfire.com, All Rights Reserved