Ferro Frit 3221

Leadless alkali borosilicate frit

OxideAnalysisFormula
CaO0.20%0.014
K2O4.13%0.175
Na2O12.60%0.811
Al2O317.66%0.691
B2O326.12%1.497
SiO239.29%2.608
Oxide Weight398.99
Formula Weight398.99
If this formula is not unified correctly please contact us.
COLE - Co-efficient of Linear Expansion 5.80
MLRG - Frit Melting Range (C) 1450F

Out Bound Links


By Tony Hansen

XML for Import into INSIGHT

<?xml version="1.0" encoding="UTF-8"?> <material name="Ferro Frit 3221" descrip="Leadless alkali borosilicate frit" searchkey="" loi="0.00" casnumber="65997-18-4"> <oxides> <oxide symbol="CaO" name="Calcium Oxide, Calcia" status="" percent="0.200" tolerance=""/> <oxide symbol="K2O" name="Potassium Oxide" status="" percent="4.130" tolerance=""/> <oxide symbol="Na2O" name="Sodium Oxide, Soda" status="" percent="12.600" tolerance=""/> <oxide symbol="Al2O3" name="Aluminum Oxide, Alumina" status="" percent="17.660" tolerance=""/> <oxide symbol="B2O3" name="Boric Oxide" status="" percent="26.120" tolerance=""/> <oxide symbol="SiO2" name="Silicon Dioxide, Silica" status="" percent="39.290" tolerance=""/> </oxides> </material>


Feedback, Suggestions

Your email address

Subject

Your Name

Message


Copyright 2003, 2008, 2015 https://digitalfire.com, All Rights Reserved